In order to make the alloy light magnesium is added. But it is added upto certain amount, exceeding 15% magnesium can cause coal dust and aluminium create spontaneous combustion under ideal condition at temperature as low as 150 degree celcius.
In order to make the alloy light magnesium is added. But it is added upto certain amount, exceeding 15% magnesium can cause coal dust and aluminium create spontaneous combustion under ideal condition at temperature as low as 150 degree celcius.