GATE MT 2011 Q4. Which one of the following refractory materials is NOT used in the BOF (LD) working lining?
GATE MT 2011 Q4. Which one of the following refractory materials is NOT used in the BOF (LD) working lining?
Share
Lost your password? Please enter your email address. You will receive a link and will create a new password via email.
Please briefly explain why you feel this question should be reported.
Please briefly explain why you feel this answer should be reported.
Please briefly explain why you feel this user should be reported.
This is because the nature of slag is basic and it is not advisable to use acidic lining of alumina.
This is because the nature of slag is basic and it is not advisable to use acidic lining of alumina.
See lessCorrect answer is option D.
Correct answer is option D.