GATE MT 2014 Q1. Which one of the following factors is NOT desirable for effective phosphorus removal in BOF steelmaking process?
GATE MT 2014 Q1. Which one of the following factors is NOT desirable for effective phosphorus removal in BOF steelmaking process?
Share
Correct answer is option C. Phosphorus can also be removed during the steel refining process. Over 90 % of the input P in the melt can be removed in the BOF. The refining capacity of the slag depends of many variables such as slag and metal compositions, lower temperature, time and intensity of slagRead more
Correct answer is option C.
Phosphorus can also be removed during the steel refining process. Over 90 % of the input P in the melt can be removed in the BOF. The refining capacity of the slag depends of many variables such as slag and metal compositions, lower temperature, time and intensity of slag/metal stirring.
See less