Sign Up Sign Up

Connect with:
Google
or use


Have an account? Sign In Now

Sign In Sign In

Connect with:
Google
or use


Forgot Password?

Don't have account, Sign Up Here

Forgot Password Forgot Password

Lost your password? Please enter your email address. You will receive a link and will create a new password via email.


Have an account? Sign In Now

Sorry, you do not have permission to ask a question, You must login to ask a question.

Connect with:
Google
or use


Forgot Password?

Need An Account, Sign Up Here

Please briefly explain why you feel this question should be reported.

Please briefly explain why you feel this answer should be reported.

Please briefly explain why you feel this user should be reported.

Sign InSign Up

Askmemetallurgy

Askmemetallurgy Logo Askmemetallurgy Logo

Askmemetallurgy Navigation

  • MCQs
    • Metallurgical Engineering mcq
    • Topic Wise mcq
    • Numericals
  • GATE Papers
  • Notes
Search
Ask A Question

Mobile menu

Close
Ask a Question
  • Home
  • Categories
  • GATE Papers
  • Recent Posts
  • Badges
  • MCQs
    • Metallurgical Engineering mcq
    • Topic Wise mcq
    • Numericals
  • GATE Papers
  • Notes
Home/Questions/Q 174743
Next
Askmemetallurgy Official
Poll
Askmemetallurgy OfficialGold
Asked: February 25, 20222022-02-25T01:34:54+05:30 2022-02-25T01:34:54+05:30In: Foundry Technology (Metal Casting)

GATE MT 2022 Q12. In green sand moulding, the casting defect resulting from the displacement of mould cavity by an oversized core is known as             

Poll Results

29.23% (A) Crush ( 19 voters )
18.46% (B) Hot tear ( 12 voters )
26.15% (C) Blow ( 17 voters )
26.15% (D) Fin ( 17 voters )
Based On 65 Votes

Participate in Poll, Choose Your Answer.

GATE MT 2022 Q12. In green sand moulding, the casting defect resulting from the displacement of mould cavity by an oversized core is known as             
GATE MT 2022 Question paper with solutionGATE MT Foundry technologyGATE MT Previous Year Questions With Solution
  • 0
  • 00
  • 169
  • 0
  • 0
Share
  • Facebook

    You must login to add an answer.

    Connect with:
    Google
    or use


    Forgot Password?

    Need An Account, Sign Up Here

    Sidebar

    Related Questions

      • On: February 25, 2022
      • Answers: 2

      GATE MT 2022 Q47

      The equilibrium microstructure of an alloy A-B consists of two phases α and β in the molar proportion 2:1. If the overall composition of the alloy is 70 mol% B and the composition of β is 90 mol%

      • On: February 25, 2022
      • Answers: 0

      GATE MT 2022 Q46

      Given the stress tensor, the maximum shear stress is     MPa (round off to the nearest integer).

      • On: February 25, 2022
      • Answers: 2

      GATE MT 2022 Q45

      Air at 300 K is passed at a mass flow rate of 1.5 kgs1  through a metallic tube of inner diameter 0.08 m. Inner wall temperature of the tube is maintained at 700 K. Temperature of the air

      • On: February 25, 2022
      • Answers: 0

      GATE MT 2022 Q44

      A cylindrical specimen of an Al alloy with diameter of 30 mm is cold extruded to  a diameter of 20 mm. If the flow behavior of the alloy is expressed by the  equation, 𝜎 = 350 𝜖0.3 MPa,

      • On: February 25, 2022
      • Answer: 1

      GATE MT 2022 Q43

      Steel plates are welded autogenously using Gas Tungsten Arc welding with an  arc heat transfer efficiency of 0.65. The first weld is made using a welding current of 200 A at an arc voltage of 18 V with

    Top Users

    Arpita Samal

    Arpita Samal

    • 7 Questions
    • 1,691 Points
    Platinum⭐
    digbijaya igit

    digbijaya igit

    • 11 Questions
    • 1,417 Points
    Platinum⭐
    Rohit.km

    Rohit.km

    • 2 Questions
    • 1,408 Points
    Platinum⭐

    Adv 120×600

    Explore

    • Home
    • Categories
    • GATE Papers
    • Recent Posts
    • Badges

    Footer

    Askmemetallurgy.com

    Askmemetallurgy is the one stop solution for all the need of a Metallurgical Engineers. Askmemetallurgy provides its users with a variety of services to help meta students from semester to his career path. Learn more.

    Legal Stuff

    • Privacy Policy
    • Terms Of Use

    Help & Services

    • FAQ
    • Contact Us

    Copyright © 2021 Askmemetallurgy.com, All rights reserved. Registration on or use of this site constitutes acceptance of our Privacy Policy
    DMCA.com Protection Status